Abstract

DRIVER 90 ALLOY is a copper-nickel alloy for use where only moderately low electrical resistance is required. The number designations refers to its specific resistivity (90 ohms/cir mil/ft) which is combined with a moderate coefficient of resistance. Its maximum recommended operating temperature is 800 F. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and heat treating. Filing Code: Cu-343. Producer or source: Wilbur B. Driver Company.