Abstract

BUNTING Alloy 932 is a cast bearing and bushing bronze. It has excellent anti-friction characteristics and load capacity. Its uses include a wide variety of industrial and automotive equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-330. Producer or source: NL Industries Inc., Bearing Division.