Abstract

ATLANTIC 13B Alloy is a silicon bronze casting alloy offering excellent castability and corrosion resistance, good machinability and medium-high strength. It is an all-purpose alloy that is suitable for gears, valve parts and marine fittings. It is especially useful in stress-corrosion environments for thin-walled parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-307. Producer or source: Atlantic Casting and Engineering Corporation.