Abstract
IN-838 is a wrought copper-15% nickel alloy with a controlled chromium addition for improved corrosion resistance in flowing sea water. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-297. Producer or source: Brass mills.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.