Abstract

OLIN STRESCON ALLOY 195 is a high-strength, high-conductivity copper alloy developed for applications in current-carrying parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-260. Producer or source: Olin Corporation, Brass Group.