Abstract

COPPER ALLOY No. 230 is a single-phase brass containing 15% zinc which is the most widely used of the low zinc brasses. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-252. Producer or source: Brass mills.