Abstract

COPPER ALLOY No. 485 is a free-cutting copper-zinc alloy having good mechanical properties and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-249. Producer or source: Brass mills.