Abstract

COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. This datasheet provides information on composition, physical properties, tensile properties, and compressive strength. and bearing strength It also includes information on corrosion resistance Filing Code: Cu-246. Producer or source: Bound Brook Bearing Corporation of America.