Elkaloy-A is a copper-base alloy having high strength and toughness coupled with high electrical and thermal conductivity. It is recommended for springs, electrical contacts and resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-198. Producer or source: Mallory Metallurgical Company.