Mueller 3770 (formerly MBCo 200 Alloy) is a free-cutting, leaded brass recommended for forgings of all kinds. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-182. Producer or source: Mueller Brass Company.