Incramet 800 is a copper-base alloy exhibiting an excellent combination of mechanical, physical and corrosion resistant properties at both room and elevated temperatures. It is recommended for glass container molds and sheet glass rolls. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-173. Producer or source: Licensees of the International Copper Research Association.