Abstract

Bohnolloy R-57 is a very strong manganese bronze recommended for parts which are subjected to heavy loads. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-148. Producer or source: Bohn Aluminum & Brass Corporation.