Abstract

Copper Alloy No. 377 is a free-machining, leaded brass recommended for forgings and pressings of all kinds. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-147. Producer or source: Brass mills.