Copper Alloy No. 710 is a cupro-nickel alloy having high creep strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low temperature performance and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-134. Producer or source: Anaconda American Brass Company.