Abstract

NI-VEE TYPE B is a precipitation hardening nickel bronze alloy suitable for constructional castings. This alloy provides the advantage of maximum strength in contact with steel or similar hard and strong coostruction material. It has improved machinability compared with Ni-Vee Type A (Alloy Digest Cu-66, August 1958). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: Cu-102. Producer or source: The International Nickel Company Inc..