Abstract

TUF-STUF 224C is a general purpose aluminum bronze for use where high strength and corrosion resistance are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-92. Producer or source: Mueller Brass Company.