Abstract

KUMANIC is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength along with excellent resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-79. Producer or source: Imperial Chemical Industries Ltd.