CUPRO-NICKEL 30% is a copper-nickel alloy having high strength, ductility and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-70. Producer or source: American Brass Company.