NI-VEE Type D is a precipitation hardening leaded-nickel bearing bronze suitable for bearings and acid-resisting castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion and wear resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-55. Producer or source: The International Nickel Company Inc.. Originally published September 1957, revised March 1962.