Abstract

MUELLER 515 is a nickel silver alloy having good resistance to corrosion, high mechanical properties, and good machining qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-54. Producer or source: Mueller Brass Company.