Abstract

DURONZE 609 ia tough silicon bronze having good resistance to wear and to corrosion. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-45. Producer or source: Bridgeport Brass Company.