Abstract

EVERDUR-1015 is a high-strength, corrosion-resistant copper-silicon alloy having good fabricating properties. It is nonmagnetic and fatigue resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-39. Producer or source: The American Brass Company.