Abstract

LUMEN 15 and 15A are deoxidized tin-bronze casting alloys recommended for worm gears and heavy duty bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on machining and joining. Filing Code: Cu-37. Producer or source: Lumen Bearing Company.