Abstract

ADMIRALTY METAL is a corrosion resistant brass alloy recommended especially for condenser tubing. It is better known as Inhibited Admiralty. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-34. Producer or source: Brass mills.