Abstract

MUELLER 600 BEARING BRONZE is a copper-base beating alloy possessing excellent hot working qualities, high mechanical properties and good resistance to wear. It is also corrosion resistant. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-17. Producer or source: Mueller Brass Company. Originally published June 1954, revised April 1965.