AMBRALOY 917 is a heat treatable aluminum bronze combining high strength with excellent resistance to corrosion. It is wear and abrasion resistant. It is also nonmagnetic and resistant to sparking. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-5. Producer or source: American Brass Company.