Lucefin Group C30, C30E, and C30R are medium-carbon, non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. C30E and C30R may also be flame or induction hardened. C30, C30E, and C30R are widely used for small, moderately stressed parts, where higher strength levels are needed than can be achieved in the lower carbon grades, and also where toughness is more important than high tensile strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-206. Producer or source: Lucefin S.p.A.