Lucefin Group C35, C35E, and C35R are medium-carbon, non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. C35E and C35R may also be flame or induction hardened. C35, C35E, and C35R are widely used for moderately stressed parts, where higher strength levels are needed than can be achieved in the lower carbon grades, and where the expense of an alloy steel is not justified. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-205. Producer or source: Lucefin S.p.A.