AncorLam is a high performance insulated particle material suitable for a variety of soft magnetic applications that require low core losses. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on powder metal forms. Filing Code: CS-194. Producer or source: Hoeganaes Corporation.