Abstract

Dogal H 700 LAD is a galvanized hot rolled steel that is microalloyed and can be cold formed. The 700 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CS-184. Producer or source: SSAB Swedish Steel Inc..