Abstract

Dogal 300 LAD, 340 LAD, 380 LAD, 420 LAD, 460 LAD and 500 LAD are high-strength low alloyed steels intended for pressing. The designation in the name is the guaranteed minimum yield strength. Dogal steels can be zinc coated. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on surface qualities as well as forming, heat treating, joining, and surface treatment. Filing Code: CS-167. Producer or source: SSAB Swedish Steel Inc..