DOGAL 200 AND DOGAL FORM mild steels can be used for applications ranging all the way from simple pressing up to advanced drawing and stretch forming. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, joining, and surface treatment. Filing Code: CS-158. Producer or source: SSAB Swedish Steel Inc.