Abstract

Ancorsteel 50 HP is a water-atomized, prealloyed low-alloy steel powder for high-performance applications. The prealloyed 0.50 wt.% Mo addition results in high compressibility and provides good response to heat treatment. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles that are then annealed to produce uniform, dependable steel powders. Ancorsteel 50 HP is an ideal base powder for a wide range of nickel-copper and chromium-manganese hybrid alloy systems. This datasheet provides information on composition and physical properties. It also includes information on powder metal forms. Filing Code: CS-153. Producer or source: Hoeganaes Corporation.