Sandvik Bioline 20AP is a high-hardness alloy with dimensional stability and excellent machining properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: CS-145. Producer or source: Sandvik Steel Company. See also Alloy Digest SA-642, January 2012.