AlgoTuf 450F is one of a full range of heat-treated plate products for construction, mining, manufacturing and military applications. This datasheet provides information on composition as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: CS-139. Producer or source: Algoma Steel Corporation Ltd.