Abstract

Cal Hi-Form 80Y100T is a dual-phase steel that offers a combination of strength and formability to permit weight reduction and cost savings in demanding manufacturing conditions. See also Inland Hi-Form, Alloy Digest SA-346, May 1978. This datasheet provides information on composition, physical properties, elasticity, tensile properties, shear and bend strength. Filing Code: CS-136. Producer or source: Ispat Inland Inc. Originally published May 1978, revised May 2003.