Abstract

SANDVIK 15N2 is strip steel for stonecutting saws and especially designed for the manufacture of diamond saw blades. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CS-134. Producer or source: Sandvik.