AISI C1117 is a low-carbon free-machining case-hardening steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: CS-14. Producer or source: Carbon and alloy steel mills.