Abstract

AKULOY RM M-1915 is a thermoplastic composite that can be used in many types of injection molded applications where polypropylene or nylon are used. This datasheet provides information on physical properties, and tensile properties as well as fracture toughness. Filing Code: Cp-17. Producer or source: AKZO Engineering Plastics.