Abstract

AVIMID N / GRAPHITE is a carbon-fiber/polyimide, high-temperature composite tooling material developed to fabricate quality parts from prepregs based on thermoplastics. This datasheet provides information on physical properties, and tensile properties as well as fracture toughness. It also includes information on high temperature performance. Filing Code: Cp-11. Producer or source: E. I. Dupont de Nemours & Company Inc..