Abstract

Hiperco 50A is an iron-cobalt-vanadium soft magnetic alloy possessing high magnetic saturation, high direct current (dc) maximum permeability, low dc coercive force, and low alternating current (ac) core loss. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on heat treating. Filing Code: CO-107. Producer or source: Carpenter.