Inconel Alloy 783 is an oxidation resistant, low expansion, nickel-cobalt-iron alloy with other additions. The alloy is a three-phase aging alloy that is of interest for close clearance control components in the aerospace arena. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: CO-95. Producer or source: Special Metals Corporation. Originally published January 1995, revised February 2004.