Abstract

STOODY 4 is a cobalt-chromium-tungsten alloy with excellent high-temperature strength and excellent resistance to corrosion. This alloy derives its high-temperature strength from the high tungsten-to-carbon ratio which allows a large percentage of tungsten to remain in solid solution. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-75. Producer or source: WRAP Division, Stoody Company.