Tantung 144 is a cast nonferrous alloy recommended for cutting tools where resistance to abrasion is paramount and where there is little or no shock or impact. This datasheet provides information on composition, physical properties, and hardness as well as creep. It also includes information on forming, heat treating, machining, and joining. Filing Code: Co-34. Producer or source: Vascoloy, Ramet Division.