Abstract

HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-29. Producer or source: Haynes Stellite Company.