Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on machining. Filing Code: CI-65. Producer or source: Charter Dura-Bar, Inc.