Abstract

MEEHANITE SC is a heat resisting iron casting alloy recommended for applications where fairly constant temperatures are involved and for exceptional resistance to growth and scaling. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as creep. It also includes information on high temperature performance as well as casting, heat treating, and machining. Filing Code: CI-27. Producer or source: Meehanite Metal Corporation.