Abstract
ADVANCER NITRIDE BONDED SILICON CARBIDE has exceptional high-temperature strength. Its oxidation resistance assures long life. It is a low-mass ceramic that is ideally suited to kiln furniture. This datasheet provides information on composition, physical properties, elasticity, and shear strength. Filing Code: Cer-11. Producer or source: Norton Company.