Abstract

SILICON NITRIDE SN-220 has found its niche in industrial applications in engine and gas turbine components. It has excellent high-temperature strength and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and bend strength as well as fracture toughness. Filing Code: Cer-4. Producer or source: Kyocera America Inc..