Westinghouse Alloy B33 is a columbium-base alloy for high temperature applications requiring moderate strength where excellent fabricability, weldability, and resistance to liquid metal corrosion are prime requisites. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cb-1. Producer or source: Westinghouse Electric Corporation.